Progress on Pellet–Cladding Interaction and Stress Corrosion Cracking: Experimentation, Modelling and Methodologies Applied to Support the Flexible Operation of Nuclear Power Plants: Report of a Technical Meeting - IAEA TECDOC Iaea
Do you have a profile? Pierakstīties
Ziemassvētku dāvanas var atgriezt līdz 31. janvārim
Saņemiet paziņojumus par jauniem Iaea izdevumiem
Pievienot savam iMusic vēlmju sarakstam
Progress on Pellet–Cladding Interaction and Stress Corrosion Cracking: Experimentation, Modelling and Methodologies Applied to Support the Flexible Operation of Nuclear Power Plants: Report of a Technical Meeting - IAEA TECDOC
Iaea
Provides an overview of pellet-cladding interaction/stress corrosion cracking (PCI/SCC) and reports on the progress made since the early 2000s, based on presentations and discussions at a related IAEA technical meeting held in October 2019.
312 pages, 13 illustrations
| Mediji | Grāmatas Paperback Book (Grāmata ar mīksto vāku un līmēto muguru) |
| Izlaists | 2021. gada 30. jūlijs |
| ISBN13 | 9789201165213 |
| Izdevēji | IAEA |
| Lapas | 312 |
| Izmēri | 150 × 220 × 10 mm · 830 g |