Formation of Hgcdte (Mct) by Electrochemical Atomic Layer Deposition: an Investigation into Bandgap Engineering - Venkatram Venkatasamy - Grāmatas - LAP LAMBERT Academic Publishing - 9783844323979 - 2011. gada 6. aprīlis
Ja vāks un nosaukums nesakrīt, pareizs ir nosaukums

Formation of Hgcdte (Mct) by Electrochemical Atomic Layer Deposition: an Investigation into Bandgap Engineering

Cena
€ 45,49
ar PVN 12%, piegādes valsts: Latvia

Pasūtīts no attālās noliktavas

Paredzamā piegāde 18. - 28. dec.
Ziemassvētku dāvanas var atgriezt līdz 31. janvārim
Saņemiet paziņojumus par jauniem Venkatram Venkatasamy izdevumiem
Pievienot savam iMusic vēlmju sarakstam

Not rated yet

HgCdTe or Mer-Cad-Tel is the most widely used Infrared material. The present study describes the growth of MCT via Electrochemical ALD, using an automated electrochemical flow cell deposition system. Deposits were characterized using X-ray diffraction (XRD), electron probe microanalysis (EPMA) and reflection absorption Fourier transform Infrared spectroscopy (FTIR). As deposited films showed a strong (111) preferred orientation. Changes in deposit composition showed the expected trend in band gaps: the more Hg the lower the band gap, but with some significant deviations. Electrochemical quartz crystal microbalance (EQCM) studies, using an automated flow cell, indicated that some deposited Cd was stripping at potentials used to deposit Hg. In addition, redox replacement of deposited Cd for Hg was evident, a function of the greater stability of Hg than Cd.

Mediji Grāmatas     Mīkstie vāki   (Grāmata ar mīksto vāku un līmēto muguru)
Izlaists 2011. gada 6. aprīlis
ISBN13 9783844323979
Izdevēji LAP LAMBERT Academic Publishing
Lapas 116
Izmēri 150 × 7 × 226 mm   ·   191 g
Valoda Vācu  

Vairāk no Venkatram Venkatasamy