Provides general descriptions of degradation mechanisms of different types of stress corrosion cracking (SCC) which are concerned with systems, structures and components in PWRs and BWRs. This publication includes examples of good practices in preventing, mitigating and repairing SCC damage and summarizes research and development programmes.