How Do Flowing Conditions Affect Copper / Aisi 304 Galvanic Corrosion?: Electrochemical Study on Heavy Lithium Bromide Brines - José García-antón - Grāmatas - LAP LAMBERT Academic Publishing - 9783844314656 - 2011. gada 1. marts
Ja vāks un nosaukums nesakrīt, pareizs ir nosaukums

How Do Flowing Conditions Affect Copper / Aisi 304 Galvanic Corrosion?: Electrochemical Study on Heavy Lithium Bromide Brines

Cena
€ 45,49

Pasūtīts no attālās noliktavas

Paredzamā piegāde . gada 27. okt. - . gada 4. nov.
Saņemiet paziņojumus par jauniem José García-antón izdevumiem
Pievienot savam iMusic vēlmju sarakstam

Not rated yet

Absorption cooling is a suitable alternative to refrigeration compression systems which use refrigerants that are responsible for the ozone layer depletion and the climate change. Despite the fact that lithium bromide is the most commonly used absorbent in absorption systems, it contains bromides, which cause corrosion problems. Additionally, the fluid flow can enhance these problems. Copper and stainless steels are widely used in the construction of absorption systems. This book provides a comprehensive study of the influence of Reynolds number (including a hydraulic circuit design)on the galvanic corrosion of the copper/AISI 304 stainless steel pair in heavy lithium bromide brines using electrochemical techniques. Results can be useful for those who develop their research in the electrochemical field, where there is a lack of studies about corrosion taking into consideration flowing conditions. Moreover, the results could be of interest for engineers who want to know the real corrosion behaviour in pipelines and to understand the novel zero resistance ammeter technique, which allows monitoring corrosion without disturbing the system under investigation and in continuous-time.

Mediji Grāmatas     Paperback Book   (Grāmata ar mīksto vāku un līmēto muguru)
Izlaists 2011. gada 1. marts
ISBN13 9783844314656
Izdevēji LAP LAMBERT Academic Publishing
Lapas 76
Izmēri 226 × 5 × 150 mm   ·   131 g
Valoda Vācu