Plasma-assisted Atomic Layer Deposition of Iii-nitride Thin Films: Growth and Characterization Çagla Özgit-akgün
Plasma-assisted Atomic Layer Deposition of Iii-nitride Thin Films: Growth and Characterization
Çagla Özgit-akgün
III-nitride compound semiconductors (AlN, GaN, InN) and their alloys have emerged as versatile and high-performance materials for a wide range of electronic and optoelectronic device applications. Although high quality III-nitride thin films can be grown at high temperatures (>1000 °C) with significant rates, deposition of these films on temperature-sensitive device layers and substrates necessitates the adaptation of low-temperature methods such as atomic layer deposition (ALD). When compared to other low-temperature thin film deposition techniques, ALD stands out with its self-limiting growth mechanism, which enables the deposition of highly uniform and conformal thin films with sub-angstrom thickness control. These unique characteristics make ALD a powerful method especially for depositing films on nanostructured templates, as well as preparing alloy thin films with well-defined compositions. This monograph reports on the development of low-temperature (?200 °C) plasma-assisted ALD processes for III-nitrides, and presents detailed characterization results for the deposited thin films and fabricated nanostructures.
| Mediji | Grāmatas Paperback Book (Grāmata ar mīksto vāku un līmēto muguru) |
| Izlaists | 2014. gada 17. marts |
| ISBN13 | 9783659208232 |
| Izdevēji | LAP LAMBERT Academic Publishing |
| Lapas | 180 |
| Izmēri | 150 × 10 × 226 mm · 286 g |
| Valoda | Vācu |
Skatīt visus Çagla Özgit-akgün
Ziemassvētku dāvanas var atgriezt līdz 31. janvārim